The Analysis of Resistance to Brittle Cracking of Tungsten Doped TiB2 Coatings Obtained by Magnetron Sputtering

Jerzy Smolik, Joanna Kacprzyńska-Gołacka, Sylwia Sowa, Artur Piasek

Coatings· Volume 10· Issue 9

Abstract

In this work, the authors present the possibility of characterization of the fracture toughness in mode I (KIC) for TiB2 and TiB2 coatings doped with different concentration of W (3%, 6% and 10%). The Young’s modulus, hardness and fracture toughness of this coatings are extracted from nanoindentation experiments. The fracture toughness was evaluated using calculation of crack length measurement. An important observation is that increasing tungsten concentration in the range 0–10% changes the microstructure of the investigated coatings: from columnar structure for TiB2 coating to nano-composite structure for Ti-B-W (10%) coating. It can be concluded that doping with concentration 10 at.% W causes an increase of the fracture toughness for the tested coatings.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Advanced materials and composites · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Łukasiewicz Research Networks–Institute for Sustainable Technology, 6/10 Pułaskiego St., 26-600 Radom, Poland

References (16)

Show source-provided references
1. (1987). ASTM G40-15 Standard Terminology Relating to Wear and Erosion, ASTM.
2. Review of fracture toughness (G, K, J, CTOD, CTOA) testing and standardization10.1016/j.engfracmech.2012.02.001 ↗
3. Elastic/plastic indentation damage in ceramics: The median/radial crack system10.1111/j.1151-2916.1980.tb10768.x ↗
4. Fracture toughness evaluation and plastic behavior law of a single crystal silicon carbide by nanoindentation10.3390/ceramics1010017 ↗
5. Determination of crack-free mechanical properties of brittle materials via single nanoindentation10.1016/j.ijsolstr.2020.01.024 ↗
6. Fracture toughness of glasses and hydroxyapatite: A comparative study of 7 methods by using Vickers indenter10.1016/j.ceramint.2016.05.030 ↗
7. Determination of fracture toughness of brittle materials by indentation10.1016/S0894-9166(15)30010-0 ↗
8. Measurement of fracture toughness by nanoindentation methods: Recent advances and future challenges10.1016/j.cossms.2015.04.003 ↗
9. A critical evaluation of indentation techniques for measuring fracture toughness: I, direct crack measurements10.1111/j.1151-2916.1981.tb10320.x ↗
10. New formula for indentation toughness in ceramics10.1007/BF01729352 ↗
11. Tungsten doped TiB2 coatings obtained by magnetron sputtering
12. Vickers indentation fracture toughness of near-nano and nanostructured WC-Co cemented carbides
13. Evaluation of fracture toughness of small volumes by means of cube-corner nanoindentation10.1016/j.scriptamat.2012.01.033 ↗
14. Microstructure, residual stress, and fracture of sputtered TiN films10.1016/j.surfcoat.2013.03.009 ↗
15. Fracture toughness enhancement of brittle nanostructured materials by spatial heterogeneity: A micromechanical proof for CrN/Cr and TiN/SiOx multilayers10.1016/j.matdes.2016.05.029 ↗
16. The effect of low titanium content on the phase composition, structure, and mechanical properties of magnetron sputtered WB2-TiB2 films10.1016/j.tsf.2018.07.042 ↗