journal article·2021-07-31Open access

Evaluation of Adhesion Properties of Hard Coatings by Means of Indentation and Acoustic Emission

Peter Drobný, David Mercier, Václav Koula, Sára Ivana Škrobáková, Ľubomír Čaplovič, Martin Sahul

Coatings· Volume 11· Issue 8

Abstract

In general, the mechanical properties of hard thin coatings are investigated using indentation methods. Material characteristics of hard coatings, such as elastic modulus and hardness, are evaluated by means of nanoindentation and an appropriate evaluation methodology. The most popular method used to obtain the coating properties required using nanoindentation is the evaluation based on the Oliver and Pharr methodology. Adhesion and wear properties can be calculated using these data. In this study, we used a novel method to evaluate the wear and adhesion of coatings. A special measuring device combined with static indentation and acoustic emission signal detection was developed to evaluate the adhesion of coatings. The device consists of a macrohardness instrumental indentation device equipped with an acoustic emission measuring gauge. It was used to investigate crack formation and adhesion of coatings deposited on different substrates using acoustic emissions data. The results using both the existing and novel methods were compared and evaluated.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research · Adhesion, Friction, and Surface Interactions

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Faculty of Material Science and Technology, Institute of Material Science, Slovak University of Technology in Bratislava, Jána Bottu 25, 917 24 Trnava, Slovakia

CRM Group-CRM, 4000 Liège, Belgium

ZD Rpety-Dakel, Ohrobecká 408/3, 142 00 Praha, Czech Republic

References (33)

Show source-provided references
1. Adhesion phenomena in bonded joints10.1016/j.ijadhadh.2012.04.007 ↗
2. Strength of adhesive contacts: Influence of contact geometry and material gradients10.1007/s40544-017-0177-3 ↗
3. Investigation of Cr(N)/DLC multilayer coatings elaborated by PVD for high wear resistance and low friction applications10.1016/j.surfcoat.2018.01.052 ↗
4. Sousa, V.F.C., and Silva, F.J.G. (2020). Recent advances in turning processes using coated tools—A comprehensive review. Metals, 10.10.3390/met10020170 ↗
5. Investigation of the fracture of very thin amorphous alumina film during spherical nanoindentation10.1016/j.tsf.2017.07.040 ↗
6. Krabbe, M. (2012). Crack Mechanisms and Crack Interaction in Thin Films, Aarhus University. Available online: https://tidsskrift.dk/me/article/view/21125/18625.
7. Fu, K., Tang, Y., and Chang, L. (2016). Toughness Assessment and Fracture Mechanism of Brittle Thin Films Under Nano-Indentation, Fracture Mechanics—Properties, Patterns and Behaviours, IntechOpen.10.5772/64117 ↗
8. Measuring mechanical properties of coatings: A methodology applied to nano-particle-filled sol–gel coatings on glass10.1016/S0927-796X(01)00040-7 ↗
9. Azizpour, A., Hahn, R., Klimashin, F.F., Wojcik, T., Poursaeidi, E., and Mayrhofer, P.H. (2019). Deformation and cracking mechanism in CrN/TiN multilayer coatings. Coatings, 9.10.3390/coatings9060363 ↗
10. Surface constrained plasticity: Oxide rupture and the yield point process10.1080/01418610108216651 ↗
11. Indentation strain burst phenomenon induced by grain boundaries in niobium10.1557/JMR.2004.0316 ↗
12. Mercier, D. (2021, July 30). PopIn Toolbox Documentation; GitHub. Available online: https://www.researchgate.net/publication/328530953_PopIn_Toolbox_documentation.
13. International Organization for Standardization (2002). ISO 14577-1, -2, -3, Metallic Materials–Instrumented Indentation Test for Hardness and Materials Parameters–Part 1: Test Method, Part 2: Verification and Calibration of Testing Machines, Part 3: Calibration of Reference Blocks, International Organization for Standardization.
14. International Organization for Standardization (2007). ISO 14577-4, Metallic Materials–Instrumented Indentation Test for Hardness and Materials Parameters–Part 4: Test Method for Metallic and Non-Metallic Coatings, ISO–International Organization for Standardization.
15. Silva, F.J.G. (2017). Nanoindentation on tribological coatings. Applied Nanoindentation in Advanced Materials, John Wiley and Sons, Ltd.10.1002/9781119084501.ch5 ↗
16. The VDI 3198 indentation test evaluation of a reliable qualitative control for layered compounds10.1016/S0924-0136(03)00300-5 ↗
17. Study of cathode current effect on the properties of CrAlSiN hard coatings deposited by LARC10.1016/j.vacuum.2017.01.029 ↗
18. High-temperature tribological properties of CrAlN, CrAlSiN and AlCrSiN coatings10.1016/j.surfcoat.2011.08.037 ↗
19. Structure and properties of CrAlSiN Nanocomposite coatings deposited by lateral rotating cathod arc10.1016/j.tsf.2010.10.022 ↗
20. PVD grown (Ti,Si,Al)N nanocomposite coatings and (Ti,Al)N/(Ti,Si)N multilayers: Structural and mechanical properties10.1016/S0257-8972(03)00323-2 ↗
21. Toughening of nanocomposite hard coatings10.1515/rams-2020-0049 ↗
22. TripleCoatings3®–New generation of PVD-coatings for cutting tools
23. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
24. Measurement of hardness and elastic modulus by instrumented indentation: Advances in understanding and refinements to methodology10.1557/jmr.2004.19.1.3 ↗
25. Tribological and mechanical properties of nanocrystalline-TiC/a-C nanocrystalline-TiC/a-C nanocomposite thin films10.1116/1.3294717 ↗
26. Hard and superhard nanocomposite coatings10.1016/S0257-8972(99)00586-1 ↗
27. Hard nanocomposite coatings: Thermal stability, oxidation resistance and toughness10.1016/j.surfcoat.2012.05.073 ↗
28. Relations between hardness, youngs modulus and elastic recovery in hard nanocomposite coatings10.1016/S0257-8972(01)01714-5 ↗
29. On the significance of the H/E ratio in wear control: A nanocomposite coating approach to optimised tribological behaviour10.1016/S0043-1648(00)00488-9 ↗
30. (1991). Verein Deutscher Ingenieure Normen, VDI 3198, VDI-Verlag.
31. Grosse, U.C.H., and Ohtsu, M. (2008). Acoustic Emission Testing, Springer. [1st ed.].10.1007/978-3-540-69972-9 ↗
32. Study of the relationship between concrete fracture energy and AE signal energy under uniaxial compression10.1061/(ASCE)MT.1943-5533.0000418 ↗
33. Acoustic emission analysis of hard coatings cracking during indentation test10.1088/1757-899X/726/1/012004 ↗