journal article·2019-12-10Open access

RETRACTED: Structure Investigation of Titanium Metallization Coating Deposited onto AlN Ceramics Substrate by Means of Friction Surfacing Process

Tomasz Chmielewski, Michał Hudycz, Arkadiusz Krajewski, Tadeusz Sałaciński, Beata Skowrońska, Rafał Świercz

Coatings· Volume 9· Issue 12
This record is marked as retracted by the source. Review the publisher’s notice before using its findings.

Abstract

The article presents selected properties of a titanium metallization coating deposited on aluminum nitride (AlN) ceramics surface by means of the friction surfacing method. Its mechanism is based on the formation of a joint between the surface of an AlN ceramics substrate and a thin Ti coating, involving a kinetic energy of friction, which is directly converted into heat and delivered in a precisely defined quantity to the resulting joint. The largest effects on the final properties of the obtained coating include the high affinity of titanium for oxygen and nitrogen and a relatively high temperature for the deposition process. The titanium metallization coating was characterized in terms of surface stereometric structure, thickness, surface morphology, metallographic microstructural properties, and phase structure. The titanium coating has a thickness ranging from 3 to 7 μm. The phase structure of the coating surface (XPS investigated) is dominated by TiNxOy with the presence of TiOx, TiN, metallic Ti, and AlN. The phase structure deeper below the surface (XRD investigated) is dominated by metallic Ti with additional AlN particles originating from the ceramic substrate due to friction by titanium tools.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Surface Treatment and Coatings · Tribology and Wear Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Warsaw University of Technology, 02-524 Warsaw, Poland

References (47)

Show source-provided references
1. Joining of AlN and graphite disks using interlayer tapes by spark plasma sintering10.1016/j.matdes.2013.09.003 ↗
2. Contact-reactive brazing of Ti3SiC2 ceramic to TC4 alloy using a Ni interlayer: Interfacial microstructure and joining properties10.1016/j.ceramint.2018.04.006 ↗
3. Optimization of hydroxyapatite synthesis and microplasma spraying of porous coatings onto titanium implants10.1515/adms-2017-0043 ↗
4. Joining of AlN with metals and alloys10.1016/S0955-2219(00)00037-6 ↗
5. Testing of flame sprayed Al2O3 matrix coatings containing TiO210.1515/amm-2016-0224 ↗
6. Effect of friction stir processing (FSP) on microstructure and hardness of AlMg10/SiC composite10.24425/bpas.2019.126530 ↗
7. Dielectric and thermal properties of AlN ceramics10.1016/j.jeurceramsoc.2006.11.023 ↗
8. Sałacinski, T., Winiarski, M., Chmielewski, T., and Swiercz, R. (2017, January 24–26). Surface finishing using ceramic fibre brush tools. Proceedings of the METAL 2017-26th International Conference on Metallurgy and Materials, Brno, Czech Republic.
9. High-performance electrical discharge machining of small hole in metallic ceramic composites
10. Skowrońska, B., Szulc, J., Chmielewski, T., Sałaciński, T., and Świercz, R. (2018, January 23–25). Properties and microstructure of hybrid PLASMA+MAG welded joints of thermomechanically treated S700MC steel. Proceedings of the METAL 2018-27th International Conference on Metallurgy and Materials, Brno, Czech Republic.
11. Kik, T., and Górka, J. (2019). Numerical simulations of laser and hybrid S700MC T-joint welding. Materials, 12.10.3390/ma12030516 ↗
12. Residual stresses determined by the modified sachs method within a gas detonation sprayed coatings of the Fe-Al intermetallic
13. Metallization of ceramic materials based on the kinetic energy of detonation waves10.1515/bpasts-2015-0051 ↗
14. Utilizing the energy of kinetic friction for the metallization of ceramics10.1515/bpasts-2015-0023 ↗
15. Brazing of alumina ceramics modified by pulsed plasma beams combined with Arc PVD treatment10.1016/S0042-207X(02)00660-7 ↗
16. Simões, S., Ramos, A.S., Viana, F., Vieira, M.T., and Vieira, M.F. (2016). Joining of TiAl to steel by diffusion bonding with Ni/Ti reactive multilayers. Metals, 6.10.3390/met6050096 ↗
17. Simões, S. (2018). Recent progress in the joining of titanium alloys to ceramics. Metals, 8.10.3390/met8110876 ↗
18. Influence of temperature of friction stir welding process with mixing-FSW-on the strength of the weld
19. Enhancing the properties of friction stir welded stainless steel joints via multi-criteria optimization10.1016/j.acme.2016.03.012 ↗
20. The effect of multiple processing on the strength of polylactide/polypropylene mixture
21. Spindle speed in friction surfacing of 316L stainless steel—How it affects the microstructure, hardness and pitting corrosion resistance10.1016/j.surfcoat.2019.01.055 ↗
22. Friction weldability of UFG 316L stainless steel
23. Fabrication of stainless steel 316 L/TiB2 composite coating via friction surfacing10.1016/j.surfcoat.2018.03.065 ↗
24. Lacki, P., Wojsyk, K., Kudla, K., and Śliwa, R.E. (2012, January 10–14). Friction welding of the bars made of aluminium and titanium alloys. Proceedings of the ECCOMAS 2012–6th European Congress on Computational Methods in Applied Science and Engineering, Vienna, Austria.
25. Morawinski, L., Chmielewski, T., Olejnik, L., Buffa, G., Campanella, D., and Fratini, L. (2018, January 23–25). Welding abilities of UFG metals. Proceedings of the 21st International ESAFORM Conference on Material Forming (ESAFORM 2018), AIP Conference Proceedings, Palermo, Italy.10.1063/1.5034885 ↗
26. The effect of surface condition on wetting of hastelloy® X by brazing filler metal of Ni-Pd-Cr-B-Si system10.1007/s11665-019-03998-0 ↗
27. Welding and joining of titanium aluminides10.3390/ma7074930 ↗
28. Characterization of microstructure and mechanical properties of Al2O3/TiAl joints vacuum-brazed with Ag-Cu-Ti+W composite filler10.1016/j.vacuum.2017.06.020 ↗
29. Interface compounds formed during the diffusion bonding of Al2O3 to Ti10.1023/A:1004815830980 ↗
30. Joining of the AMC composites reinforced with Ti3Al intermetallic particles by resistance butt welding10.1515/amm-2016-0143 ↗
31. Presz, W., and Cacko, R. (2017, January 24–26). Application of complex micro-die for extrusion of micro-rivets for micro-joining. Proceedings of the METAL 2017-26th International Conference on Metallurgy and Materials, Brno, Czech Republic.
32. Influence of micro-rivet manufacturing process on quality of micro-joints10.1063/1.3589571 ↗
33. Moravec, J., Novakova, I., Sobotka, J., and Kik, T. (2018, January 30). Possibilities of using interlayers during diffusion welding of Ti Gr2 and AlSI 316L. Proceedings of the MATEC Web of Conferences–3rd Innovative Technologies in Engineering Production, Bojnice, Slovakia.10.1051/matecconf/201824401013 ↗
34. Swiercz, R., and Oniszczuk-Swiercz, D. (2017). Experimental investigation of surface layer properties of high thermal conductivity tool steel after electrical discharge machining. Metals, 7.10.3390/met7120550 ↗
35. Structure and properties of coatings made with self shielded cored wire
36. Winczek, J. (2017). Modeling of temperature field during multi-pass gmaw surfacing or rebuilding of steel elements taking into account the heat of the deposit metal. Appl. Sci., 7.10.3390/app7010006 ↗
37. Tomków, J., Fydrych, D., and Rogalski, G. (2019). Role of bead sequence in underwaterwelding. Materials, 12.10.3390/ma12203372 ↗
38. Friction surfacing—A review10.1016/j.jmatprotec.2013.12.008 ↗
39. Investigations of interface properties in copper-silicon carbide composites10.1515/amm-2017-0200 ↗
40. Ion implanted inconell alloy–SIMS and GDMS depth profile analysis10.1002/sia.5154 ↗
41. Deposition of thin hydroxyapatite films by 335 nm Nd:YAG laser ablation
42. Brazing joining of Ti3AlC2 ceramic and 40Cr steel based on Ag-Cu-Ti filler metal10.1016/j.jmatprotec.2017.08.017 ↗
43. Development and application of a ternary Ti-Al-N interatomic potential for Ti2AlN/TiAl composite10.1016/j.jallcom.2018.02.168 ↗
44. Relationship between surface properties (roughness, wettability) of titanium and titanium alloys and cell behavior10.1016/S0928-4931(03)00033-X ↗
45. Heo, H., Joung, H., Jung, K., and Kang, C.-Y. (2018). Formation of interfacial reaction layers in Al2O3/SS 430 brazed joints using Cu-7Al-3.5 Zr alloys. Metals, 8.10.3390/met8120990 ↗
46. Active metal brazing of silicon nitride ceramics using a Cu-based alloy and refractory metal interlayers10.1016/j.ceramint.2015.12.087 ↗
47. Ultrasonic-assisted brazing of sapphire with high strength Al-4.5Cu-1.5Mg alloy10.1016/j.ceramint.2015.02.149 ↗