Abstract

Ceramic coating is an effective method for improving the erosion resistance of a material, particularly for titanium alloys. In this study, a TiN/ZrN (ceramic/ceramic) nanoscale multilayer coating is designed and prepared on the Ti6Al4V titanium alloy surface by the physical vapor deposition (PVD) process. The cross-sectional microstructure and phase composition are measured using SEM and XRD, respectively. The hardness, elastic modulus, and adhesion of the coating are measured by the nano-indentation and scratch method. The erosion test is conducted at a 45° angle with 100 m/s velocity using self-developed erosion equipment. The erosion resistance mechanisms of both the substrate and the coating are revealed more intuitively through a single sand particle impact test. The results show that the erosion resistance rate of the coating is 15.5 times higher than that of the titanium alloy substrate. The damage mechanisms of material removal of the coating include crack deflection, crack branching, and succeeding interaction between them when suffering an impacting load. These cracks are started from the droplets and the stress concentrations on the coating surface during the preparation of coating. They are the primary reasons for the decrease in the erosion resistance of the coating. This research is important for the optimization of the erosion-resistant coating structure.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Erosion and Abrasive Machining · Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

State Key Laboratory for Manufacturing Systems Engineering, Xi’an Jiaotong University, Xi’an 710049, China

Science and Technology on Plasma Dynamics Laboratory, Air Force Engineering University, Xi’an 710038, China

References (34)

Show source-provided references
1. Erosive and sliding wear of polybenzimidazole at elevated temperatures10.1007/s10853-015-9381-6 ↗
2. Particle Diameter on Erosion Resistance of Dust Removing and Washing Machine
3. Uncertainty Quantification in Erosion Predictions using Data Mining Methods10.1016/j.wear.2018.05.009 ↗
4. Kumar, K., Kumar, S., Singh, G., Singh, J.P., and Singh, J. (2017). Erosion Wear Investigation of HVOF Sprayed WC-10Co4Cr Coating on Slurry Pipeline Materials. Coatings, 7.10.3390/coatings7040054 ↗
5. Alloy Design and Application Expectation of a New Generation 600 °C High Temperature Titanium Alloy
6. Erosion wear of CrN, TiN, CrAlN, and TiAlN PVD nitride coatings10.1016/j.ijrmhm.2012.03.002 ↗
7. High velocity erosion of CVD diamond coatings by diamond particles10.1016/j.diamond.2018.02.007 ↗
8. Structural, mechanical, and sand erosion properties of TiN/Zr/ZrN multilayer coatings10.1016/j.vacuum.2015.09.026 ↗
9. High-quality diamond film deposition on a titanium substrate using the hot-filament chemical vapor deposition method10.1016/j.diamond.2006.12.016 ↗
10. CVD nanocrystalline diamond coatings on Ti alloy: A synchrotron-assisted interfacial investigation10.1016/j.matchemphys.2012.02.043 ↗
11. FE modelling of surface stresses in erosion-resistant coatings under single particle impact10.1016/j.wear.2006.04.009 ↗
12. Study on the erosion characteristics of boride coatings by finite element analysis10.1016/j.surfcoat.2017.10.042 ↗
13. Fracture observation of polycrystalline diamond film under indentation test10.1016/j.diamond.2004.08.003 ↗
14. Multilayer cracking resistance in bending10.1016/S0257-8972(97)00290-9 ↗
15. Effect of substrate preheating treatment on the microstructure and ultrasonic cavitation erosion behavior of plasma-sprayed YSZ coatings10.1016/j.ultsonch.2018.04.004 ↗
16. High temperature particulate erosion of plasma sprayed YSZ versus selected powder characteristics and plasma torch designs10.1016/S0257-8972(99)00335-7 ↗
17. Improvement of adhesion and cohesion in plasma-sprayed ceramic coatings by heterogeneous modification of nonbonded lamellar interface using high strength adhesive infiltration10.1007/s11666-012-9831-5 ↗
18. Relationship between particle erosion and lamellar microstructure for plasma-sprayed alumina coatings10.1016/j.wear.2005.07.006 ↗
19. Sintering-induced delamination of thermal barrier coatings by gradient thermal cyclic test10.1111/jace.14713 ↗
20. Non-destructive evaluation of delamination in ceramic thin films on metal substrates by scanning electron microscopy10.1016/S0040-6090(00)01904-0 ↗
21. Rao, J., Sharma, A., and Rose, T. (2017). Titanium aluminium nitride and titanium boride multilayer coatings designed to combat tool wear. Coatings, 8.10.3390/coatings8010012 ↗
22. Plotnikov, S.V., Pogrebnyak, A.D., Tleukenov, Y.O., and Erdybaeva, N.K. (2016, January 5–9). Functional properties of multilayer vacuum-arc TiN/ZrN coatings. Proceedings of the IOP Conference Series-Materials Science and Engineering, Tomsk, Russia.10.1088/1757-899X/110/1/012056 ↗
23. Nanomechanical properties of TiN/ZrN multilayers prepared by pulsed laser deposition10.1016/j.matpr.2016.04.052 ↗
24. Effect of modulation structure on the growth behavior and mechanical properties of TiN/ZrN multilayers10.1016/j.surfcoat.2006.07.132 ↗
25. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
26. Dependent Effect of Particle Size on Erosion Wear Mechanism of TC4 Titanium Alloy
27. On the significance of the H/E, ratio in wear control: A nanocomposite coating approach to optimised tribological behaviour10.1016/S0043-1648(00)00488-9 ↗
28. Mechanical, tribological and erosion behaviour of super-elastic hard Ti–Si–C coatings prepared by PECVD10.1016/j.surfcoat.2010.07.098 ↗
29. Effect of Residual Contact Stresses on Mirror-Flow-Size Relations10.1111/j.1151-2916.1980.tb10747.x ↗
30. Adhesion of reactive magnetron sputtered TIN x, and TIC y, coatings to AISI H13 tool steel10.1016/j.surfcoat.2007.07.073 ↗
31. Measurement of hardness of superhard films by microindentation10.1016/S0921-5093(02)00194-6 ↗
32. High velocity solid particle erosion behaviour of CVD boron carbide on tungsten carbide10.1016/j.wear.2004.06.005 ↗
33. Erosive wear behaviour of thick chemical vapour deposited diamond coatings10.1016/S0043-1648(98)00379-2 ↗
34. Effect of erodent hardness on erosion of brittle materials10.1016/0043-1648(88)90180-9 ↗