Recent Progress in Precision Machining and Surface Finishing of Tungsten Carbide Hard Composite Coatings
Source abstract
Abstract
Owing to their high hardness, fracture toughness and oxidation resistance, tungsten carbide (WC) coatings are extensively deposited on parts that operate in demanding applications, necessitating wear, erosion, and corrosion resistance. The application of thick and hard WC coatings has an inevitable effect on the original dimensions of the parts, affecting the geometrical tolerances and surface roughness. The capability of achieving a sub-micron surface finish and adhere to tight geometrical tolerances accurately and repeatably is an important requirement, particularly with components that operate in high-precision sliding motion. Meeting such requirements through conventional surface finishing methods, however, can be challenging due to the superior mechanical and tribological properties of WC coatings. A brief review into the synthesis techniques of cemented and binderless WC coatings is presented together with a comprehensive review into the available techniques which are used to surface finish WC-based coatings with reference to their fundamental mechanisms and capabilities to process parts with intricate and internal features. The binderless WC/W coating considered in this work is deposited through chemical vapour deposition (CVD) and unlike traditional cemented carbide coatings, it has a homogenous coating structure. This distinctive characteristic has the potential of eliminating key issues commonly encountered with machining and finishing of WC-based coatings. Here, six contact and non-contact surface finishing techniques, include diamond turning, precision grinding, superfinishing, vibratory polishing, electrical discharge machining, and electropolishing are discussed along with their current use in industry and limitations. Key challenges in the field are highlighted and potential directions for future investigation, particularly on binderless WC coatings, are proposed herein.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Advanced materials and composites · Advanced Surface Polishing Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Surface Engineering and Precision Institute, School of Aerospace, Transport and Manufacturing, Cranfield University, Cranfield MK43 0AL, UK
Hardide Coatings Plc, Bicester OX26 5AH, UK
References (100+)
Show source-provided references
1. Hoornaert, T., Hua, Z.K., and Zhang, J.H. (2009). Hard wear-resistant coatings: A review. Adv. Tribol., 774–779.10.1007/978-3-642-03653-8_257 ↗
2. Historical developments and new trends in tribological and solid lubricant coatings10.1016/j.surfcoat.2003.10.022 ↗
3. Galling resistance of nanostructured CVD tungsten/tungsten carbide coatings10.1088/2051-672X/ab1535 ↗
4. Hull, R., Chennupati, J., Richard, M.O., and Jürgen Parisi, Z.M.W. (2013). Tungsten Carbides Structure, Properties and Application in Hardmetals, Springer.
5. A review of the present state of art in hard coatings grown from the vapor phase10.1116/1.574062 ↗
6. Hardness and Young’s modulus of high-quality cubic boron nitride films grown by chemical vapor deposition10.1063/1.1534625 ↗
7. Sliding wear of conventional and nanostructured cemented carbides10.1016/S0043-1648(96)07423-6 ↗
8. Ashby, M.F. (2009). The CES EduPack Resource Booklet 2: Material and Process Selection Charts, Granta Des. Limited.
9. Samuel, J.S., and Roy, W.R. (1972). The Science of Ceramic Machining and Surface Finishing.
10. OHSA (2013). Controlling Hexavalent Chromium Exposures during Electroplating.
11. (2020, July 23). ECHA Substances Restricted under REACH. Available online: https://echa.europa.eu/substances-restricted-under-reach.
12. A review of theories of metal removal in grinding10.1243/JMES_JOUR_1969_011_050_02 ↗
13. Grinding characteristics of cBN-WC-10Co composites10.1016/j.ceramint.2017.09.040 ↗
14. Electrochemical machining of hard metals—WC/Co as example10.1179/1743290113Y.0000000062 ↗
15. Experimental study of the diamond turning characteristics of tungsten carbide (Co 0.5%) when using a chamfered diamond bite10.3938/jkps.61.1390 ↗
16. Zhang, Y.G., Sun, W.C., Ma, M., Liu, X.J., Dong, Y.R., Zi, J.Y., and Zhou, Q.X. (2019). Electrodeposition, microstructure and property of Co-WC composite coatings. Mater. Res. Express, 6.10.1088/2053-1591/ab66fe ↗
17. Mechanical and tribological evaluation of PVD WC/C coatings10.1016/S0257-8972(98)00821-4 ↗
18. Grinding of WC—Co hardmetals10.1016/S0043-1648(00)00561-5 ↗
19. High efficiency chemical assisted nanofinishing of HVOF sprayed WC-Co coating10.1016/j.surfcoat.2017.11.041 ↗
20. Kane, S.N., Mishra, A., and Dutta, A.K. (2016). Preface: International conference on recent trends in physics (ICRTP 2016). J. Phys. Conf. Ser., 755.10.1088/1742-6596/755/1/011001 ↗
21. Surface analysis of WC-5 % Co cemented tungsten carbide cutting insert after plunge-face grinding10.1007/s00170-020-05382-y ↗
22. Improving the wear behavior of WC-CoCr-based HVOF coating by surface grinding10.1007/s11665-009-9354-5 ↗
23. Grinding effects on surface integrity and mechanical strength of WC-Co cemented carbides10.1016/j.procir.2014.04.044 ↗
24. Microstructural design of hard coatings10.1016/j.pmatsci.2006.02.002 ↗
25. Sobha Jayakrishnan, D. (2012). Electrodeposition: The versatile technique for nanomaterials. Corrosion Protection and Control Using Nanomaterials, Woodhead Publishing Limited.10.1533/9780857095800.1.86 ↗
26. Electrodeposition of Ni/WC nano composite in sulfate solution10.1016/j.matchemphys.2011.04.053 ↗
27. Effect of cobalt content on wear and corrosion behaviors of electrodeposited Ni-Co/WC nano-composite coatings10.1166/jnn.2013.6025 ↗
28. Influence of SiC+WC addition to Cr(VI) bath on corrosion behaviour of coatings in sulphate solution10.1179/174591908X371159 ↗
29. Robust Ni/WC superhydrophobic surfaces by electrodeposition10.1039/C7RA08535D ↗
30. A review of nanostructured thin films for gas sensing and corrosion protection A review of nanostructured thin films for gas sensing and corrosion protection10.13171/mjc7618111916hs ↗
31. Yuan, Y., Yang, L., Liu, Z., and Chen, Q. (2018). High power impulse magnetron sputtering and its applications. Plasma Sci. Technol., 20.10.1088/2058-6272/aa9e48 ↗
32. Zhang, H., Cherng, J.S., and Chen, Q. (2019). Recent progress on high power impulse magnetron sputtering (HiPIMS): The challenges and applications in fabricating VO2 thin film. AIP Adv., 9.10.1063/1.5084031 ↗
33. Effect of substrate bias on microstructure and mechanical properties of WC-DLC coatings deposited by HiPIMS10.1016/j.surfcoat.2018.07.088 ↗
34. Thermal Spray of Cemented Carbide Coatings in Off-Angle Spraying: Correlations Between Process, Coating Features/Characteristics and Performance10.1007/s11666-018-0761-8 ↗
35. Tobergte, D.R., and Curtis, S. (2004). Handbook of Thermal Spray Technology, ASM International. [1st ed.].
36. Thermal spray maps: Material genomics of processing technologies10.1007/s11666-013-9970-3 ↗
37. Microstructures and tribological properties of ferrous coatings deposited by APS (Atmospheric Plasma Spraying) on Al-alloy substrate
38. Study of thermal expansion and thermal conductivity of cemented WC-Co composite10.1016/j.ijrmhm.2014.06.009 ↗
39. Wood, L. (2020, July 23). Tungsten Carbide Market by Value & Volume, 2014–2019 & 2020–2024. Available online: https://www.globenewswire.com/news-release/2020/02/17/1985770/0/en/Tungsten-Carbide-Market-by-Value-Volume-2014-2019-2020-2024.html.
40. Verdian, M.M. (2016). Finishing and Post-Treatment of Thermal Spray Coatings, Elsevier Ltd.10.1016/B978-0-12-803581-8.09200-6 ↗
41. Pierson, H.O. (1992). Handbook of Chemical Vapor Deposition Principles, Technology and Applications, Noyes Publications/William Andrew Publishing.
42. An Overview of Production and Development of Ceramic Membranes
43. Thick nano-structured CVD coating HARDIDE as enabler for engineering systems in extreme wear and erosion conditions
44. Fotovvati, B., Namdari, N., and Dehghanghadikolaei, A. (2019). On coating techniques for surface protection: A review. J. Manuf. Mater. Process., 3.10.3390/jmmp3010028 ↗
45. Surface & Coatings Technology Optimizing HVOF spray process parameters to attain minimum porosity and maximum hardness in WC-10Co-4Cr coatings10.1016/j.surfcoat.2014.03.022 ↗
46. An investigation on the mechanical properties of the hard chromium layer deposited by brush plating process on AISI H13 steel
47. Comparison of plasma-sprayed alumina coatings by RF and DC plasma spraying10.1007/BF02648529 ↗
48. Tribological testing of some potential PVD and CVD coatings for steel wire drawing dies10.1016/j.wear.2011.06.020 ↗
49. Deposition of well adhering cBN films up to 2 μm thickness by B-C-N gradient layer system10.1016/S0040-6090(00)01364-X ↗
50. Characterization of vanadium carbide coating deposited by borax salt bath process10.12989/amr.2012.1.3.233 ↗
51. Structural, mechanical, tribological, and corrosion properties of a-SiC:H coatings prepared by PECVD10.1016/j.surfcoat.2010.03.031 ↗
52. The role of PVD TiN coating in wear behaviour of aluminium extrusion die10.1016/S0043-1648(98)00160-4 ↗
53. Zhu, Z., and Jiang, Q. (2015, January 11–13). Research on precision and ultra-precision machining technology development. Proceedings of the International Conference on Intelligent Systems Research and Mechatronics Engineering, Zhengzhou, China.10.2991/isrme-15.2015.451 ↗
54. Leach, R.K. (2001). The Measurement of Surface Texture Using Stylus Instruments., National Physical Laboratory.
55. Smith, G.T. (2002). Industrial Metrology Surfaces and Roundness, Springer.10.1007/978-1-4471-3814-3 ↗
56. Simmons, C.H., Maguire, D.E., and Phelps, N. (2009). Geometrical tolerancing and datums. Man. Eng. Draw., 159–167.10.1016/B978-0-7506-8985-4.00020-6 ↗
57. Dimensioning and tolerancing of coated parts
58. Weiss, P.R. (1993). A Discussion of Scientific Methods for Setting Manufacturing Tolerances, University of Wisconsin.
59. Electrochemical mechanical polishing technology: Recent developments and future research and industrial needs10.1007/s00170-015-8119-6 ↗
60. Yip, A. (2014). Factors Affecting Surface Topography in Diamond Turning. [Ph.D. Thesis, McMaster University].
61. Mechanism for material removal in diamond turning of reaction-bonded silicon carbide10.1016/j.ijmachtools.2008.12.007 ↗
62. Experimental study of surface roughness on a processed detail of tungsten carbide by using a grinding device on a diamond turning machine
63. Fundamental aspects and recent developments in electropolishing10.1016/j.ijmachtools.2019.01.001 ↗
64. Ductile mode single point diamond turning (SPDT) of binderless tungsten carbide molds
65. International Journal of Mechanical Sciences Tool interference at workpiece centre in single-point diamond turning10.1016/j.ijmecsci.2018.10.057 ↗
66. Da Motta Gonçalves, A., Duduch, J.G., Jasinevicius, R.G., Montanari, L., Porto, A.J.V., and Chao, C.L. (2011, January 23–27). Single point diamond turning of tungsten carbide. Proceedings of the 11th EuspenInternational Conference, Como, Italy.
67. Influencing factors and theoretical modeling methods of surface roughness in turning process: State-of-the-art10.1016/j.ijmachtools.2018.02.001 ↗
68. Design optimization of cutting parameters for turning operations based on the Taguchi method10.1016/S0924-0136(98)00079-X ↗
69. Effect of plastic side flow on surface roughness in micro-turning process10.1016/j.ijmachtools.2005.11.014 ↗
70. He, C., and Zong, W. (2019). Influencing factors and theoretical models for the surface topography in diamond turning process: A review. Micromachines, 10.10.3390/mi10050288 ↗
71. Influence of the composition of WC-based cermets on manufacturability by wire-EDM10.1016/S1526-6125(07)00007-2 ↗
72. Balasubramaniam, R., Sarepaka, R.V., and Subbiah, S. (2017). Diamond Turn Machining: Thoery and Practice, CRC Press Taylor & Francis Froup. [1st ed.].10.1201/9781315155937 ↗
73. Li, Z., Jin, G., Fang, F., Gong, H., and Jia, H. (2018). Ultrasonically assisted single point diamond turning of optical mold of tungsten carbide. Micromachines, 9.10.3390/mi9020077 ↗
74. Zou, L., Huang, Y., Zhou, M., and Xiao, G. (2017). Thermochemical wear of single crystal diamond catalyzed by ferrous materials at elevated temperature. Crystals, 7.10.3390/cryst7040116 ↗
75. Rhorer, R.L., and Evans, C.J. (2010). Fabrication of optics by diamond turning. Handbook of Optics, McGraw-Hill.
76. Chemical aspects of tool wear in single point diamond turning10.1016/0141-6359(95)00019-4 ↗
77. Predictive modeling of transition undeformed chip thickness in ductile-regime micro-machining of single crystal brittle materials10.1016/j.jmatprotec.2008.07.036 ↗
78. Analysis on ductile mode processing of binderless, nano crystalline tungsten carbide through ultra precision diamond turning10.1016/j.jmatprotec.2011.12.010 ↗
79. Elliptical vibration cutting of tungsten alloy molds for optical glass parts
80. Ultra-precision grinding10.1016/j.cirp.2010.05.001 ↗
81. High-performance grinding—A review10.1016/j.jmatprotec.2005.04.010 ↗
82. Theoretical and experimental investigation of a tool path control strategy for uniform surface generation in ultra-precision grinding10.1007/s00170-019-03852-6 ↗
83. Ding, W., Zhang, L., Li, Z., Zhu, Y., and Su, H. (2017). Review on grinding-induced residual stresses in metallic materials. Int. J. Adv. Manuf. Technol., 2939–2968.10.1007/s00170-016-8998-1 ↗
84. Analysis of the transitional temperature for tensile residual stress in grinding10.1016/S0924-0136(00)00692-0 ↗
85. Venkastesh, V.C., and Sudin, I. (2007). Precision Engineering, Tata McGraw-Hill Publishing.
86. Analysis of the performance of superabrasive and alumina grinding wheels with different bonds and machining conditions10.1590/S1516-14392003000200020 ↗
87. Thermal Analysis of Grinding10.1016/j.cirp.2007.10.005 ↗
88. Abang Kamaruddin, A.M.N., Hosokawa, A., Ueda, T., Furumoto, T., and Koyano, T. (2015, January 18–22). Cutting performance of CBN and diamond tools in dry turning of cemented carbide. Proceedings of the 8th International Conference on Leading Edge Manufacturing in 21st Century, LEM, Kyoto, Japan.10.1299/jsmelem.2015.8._0508-1_ ↗
89. Characterization and modelling of the residual stresses induced by belt finishing on a AISI52100 hardened steel10.1016/j.jmatprotec.2007.12.133 ↗
90. Experimental investigation of methods to enhance stock removal for superfinishing
91. Forces and specific energy in superfinishing of hardened steel10.1016/S0007-8506(07)60820-8 ↗
92. Aircraft engineering and aerospace technology: 75th anniversary10.1108/aeat.2004.12776baf.001 ↗
93. Errichello, R. (2020, June 29). Case Study Another Perspective: False Brinelling and Fretting Corrosion. Available online: https://www.stle.org/images/pdf/STLE_ORG/BOK/LS/Bearings/Another%20Prospective_False%20Brinelling%20and%20Fretting%20Corrosion_tlt%20article_April04.pdf.
94. Contact mechanics of superfinishing10.1115/1.555374 ↗
95. Lepadatescu, B., and Buzatu, C. (2012). Studies and researches regarding a mathematical model of superfinishing manufacturing process. Recent Adv. Mech. Eng. Autom. Control Stud., 151–157.
96. Schmitt, R. (2014). CIRP Encyclopedia of production engineering. Int. Acad. Prod. Eng., 1085–1220.10.1007/978-3-642-20617-7_6595 ↗
97. Uhlmann, E., Spur, G., and Kleinschnitker, M. (2015). Honing and Superfinishing, Elsevier Inc.. [2nd ed.].10.1016/B978-1-4557-7858-4.00005-4 ↗
98. Porous Fine CBN Stones for High Removal Rate Superfinishing10.1016/S0007-8506(07)62328-2 ↗
99. El-Hofy, H.A.-G. (2013). Fundamentals of Machining Processes: Conventional and Nonconventional Processes, CRC Press.
100. Darmann Abrasive Products The Art of Superfinishing, Darmann Abrasive Products, Darmann Abrasive Products Inc.