journal article·2020-09-25Open access

Resistance of PVD Coatings to Erosive and Wear Processes: A Review

Alicja Krella

Coatings· Volume 10· Issue 10

Abstract

Due to the increasing maintenance costs of hydraulic machines related to the damages caused by cavitation erosion and/or erosion of solid particles, as well as in tribological connections, surface protection of these components is very important. Up to now, numerous investigations of resistance of coatings, mainly nitride coatings, such as CrN, TiN, TiCN, (Ti,Cr)N coatings and multilayer TiN/Ti, ZrN/CrN and TN/(Ti,Al)N coatings, produced by physical vapor deposition (PVD) method using different techniques of deposition, such as magnetron sputtering, arc evaporation or ion plating, to cavitation erosion, solid particle erosion and wear have been made. The results of these investigations, degradation processes and main test devices used are presented in this paper. An effect of deposition of mono- and multi-layer PVD coatings on duration of incubation period, cumulative weight loss and erosion rate, as well as on wear rate and coefficient of friction in tribological tests is discussed. It is shown that PVD coating does not always provide extended incubation time and/or improved resistance to mentioned types of damage. The influence of structure, hardness, residence to plastic deformation and stresses in the coatings on erosion and wear resistance is discussed. In the case of cavitation erosion and solid particle erosion, a limit value of the ratio of hardness (H) to Young’s modulus (E) exists at which the best resistance is gained. In the case of tribological tests, the higher the H/E ratio and the lower the coefficient of friction, the lower the wear rate, but there are also many exceptions.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research · High-Temperature Coating Behaviors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Institute of Fluid Flow Machinery, Polish Academy of Sciences, Fiszera 14, 80-231 Gdansk, Poland

References (100+)

Show source-provided references
1. Hydro-abrasive erosion in hydro turbines: A review10.1080/15435075.2018.1431546 ↗
2. Lee, J., Lee, S., Han, H.N., and Kim, W. (2020). Yttrium Oxyfluoride Coatings Deposited by Suspension Plasma Spraying Using Coaxial Feeding. Coatings, 10.10.3390/coatings10050481 ↗
3. Effect of spraying powder characteristics on mechanical and thermal shock properties of plasma-sprayed YSZ thermal barrier coating10.1016/j.surfcoat.2020.125913 ↗
4. Sprayed WC-12Co on ZE41 Magnesium Alloy10.3390/coatings10050502 ↗
5. Synergistic effect of ultrasonic cavitation erosion and corrosion of WC-CoCr and FeCrSiBMn coatings prepared by HVOF spraying10.1016/j.ultsonch.2016.02.011 ↗
6. Bouzakis, E. (2020). Fatigue Endurance Assessment of DLC Coatings on High-Speed Steels at Ambient and Elevated. Coatings, 10.10.3390/coatings10060547 ↗
7. Growth process and grain boundary defects in Er doped BaTiO3 processed by EB-PVD: A study by XRD, FTIR, SEM and AFM10.1016/j.apsusc.2019.07.003 ↗
8. Microstructure and mechanical behavior of arc-evaporated Cr-N coatings10.1016/S0257-8972(99)00019-5 ↗
9. Micro-nano multilayer structure design and solid particle erosion resistance performance of CrAlNx/CrAlN coating10.1016/j.vacuum.2019.109064 ↗
10. Corrosion and wear protection of mild steel substrates by innovative PVD coatings10.1016/j.surfcoat.2020.125659 ↗
11. CrCN/CrN ta-C multilayer coating for applications in wood processing10.1016/j.triboint.2012.07.006 ↗
12. Zhou, H., Liu, H.Y., Fu, K., Yuan, H., Du, X., and Mai, Y.W. (2019). Numerical simulation of failure of composite coatings due to thermal and hygroscopic stresses. Coatings, 9.10.3390/coatings9040243 ↗
13. Nadolny, K., Kaplonek, W., Sutowska, M., Sutowski, P., Myśliński, P., and Gilewicz, A. (2020). Experimental studies on durability of PVD-based CrCN/CrN-Coated cutting blade of planer knives used in the pine wood planing process. Materials, 13.10.3390/ma13102398 ↗
14. Paiva, J.M., Shalaby, M.A.M., Chowdhury, M., Shuster, L., Chertovskikh, S., Covelli, D., Junior, E.L., Stolf, P., Elfizy, A., and Bork, C.A.S. (2017). Tribological and wear performance of carbide tools with TiB2 PVD coating under varying machining conditions of TiAl6V4 aerospace alloy. Coatings, 7.10.3390/coatings7110187 ↗
15. Erosion and Abrasion Resistance, Mechanical Properties, and Structure of the TiN, Ti–Cr–Al–N and Cr–Al–Ti–N Coatings Deposited by CFUBMS10.1134/S2070205119050125 ↗
16. Damage evolution and mechanism of TiN/Ti multilayer coatings in sand erosion condition10.1016/j.surfcoat.2018.08.062 ↗
17. Microstructural Characterization and Room-Temperature Erosion Behavior of As-Deposited SPS, EB-PVD and APS YSZ-Based TBCs10.1007/s11666-018-0763-6 ↗
18. Mechanical properties, sliding wear and solid particle erosion behaviors of plasma enhanced magnetron sputtering CrSiCN coating systems10.1016/j.wear.2014.11.008 ↗
19. Tribological properties of nanostructured TiAlN/W2N multilayer coating produced by PVD10.1016/j.wear.2019.04.021 ↗
20. Azizpour, A., Hahn, R., Klimashin, F.F., Wojcik, T., Poursaeidi, E., and Mayrhofer, P.H. (2019). Deformation and cracking mechanism in CrN/TiN multilayer coatings. Coatings, 9.10.3390/coatings9060363 ↗
21. Investigating the high frequency fatigue failure mechanisms of mono and multilayer PVD coatings by the cyclic impact tests10.1016/j.surfcoat.2018.03.101 ↗
22. Erosive wear behavior of Ti/Ti(V,Zr)N multilayered PVD coatings for Ti-6Al-4V alloy10.1016/j.wear.2018.11.016 ↗
23. Structural, mechanical, and sand erosion properties of TiN/Zr/ZrN multilayer coatings10.1016/j.vacuum.2015.09.026 ↗
24. Composite cavitation resistant PVD coatings based on NiTi thin films10.1016/j.matdes.2016.08.054 ↗
25. Krella, A.K., Czyżniewski, A., Gilewicz, A., and Gajowiec, G. (2020). Experimental Study of the Influence of Deposition of Multilayer CrN/CrCN PVD Coating on Austenitic Steel on Resistance to Cavitation Erosion. Coatings, 10.10.3390/coatings10050487 ↗
26. Film thickness effect on texture and residual stress sign transition in sputtered TiN thin films10.1016/j.ceramint.2017.06.050 ↗
27. Experimental studies of the effect of Ti interlayers on the corrosion resistance of TiN PVD coatings by using electrochemical methods10.1016/j.corsci.2018.01.010 ↗
28. Zlamal, T., Mrkvica, I., Szotkowski, T., and Malotova, S. (2019). The influence of surface treatment of PVD coating on its quality and wear resistant. Coatings, 9.10.3390/coatings9070439 ↗
29. Enhancement of cavitation erosion resistance of 316 L stainless steel by adding molybdenum10.1016/j.ultsonch.2016.10.015 ↗
30. Zhang, L., Liu, Y.H., Luo, K.Y., Zhang, Y.K., Zhao, Y., Huang, J.Y., Wu, X.D., and Zhou, C. (2018). Tensile property of ANSI 304 stainless steel weldments subjected to cavitation erosion based on treatment of laser shock processing. Materials, 11.10.3390/ma11050805 ↗
31. On the fatigue behavior of an AISI 316L stainless steel coated with a PVD TiN deposit10.1016/j.surfcoat.2003.07.003 ↗
32. Fatigue properties of a SAE 4340 steel coated with TiCN by PAPVD10.1016/j.ijfatigue.2006.05.003 ↗
33. Influence of Ti/TiN bilayered and multilayered films on the axial fatigue performance of Ti46Al8Nb alloy10.1016/j.tsf.2010.10.025 ↗
34. Degradation of TiN coatings under cyclic loading10.1016/j.actamat.2004.03.022 ↗
35. Variables affecting the fatigue resistance of PVD-coated components10.1016/j.ijfatigue.2005.06.011 ↗
36. Influence of single-and multilayer TiN films on the axial tension and fatigue performance of AISI 1045 steel10.1016/S0040-6090(98)00880-3 ↗
37. Evaluation on the wear, tension and fatigue behavior of various PVD coated materials10.1016/S0167-577X(97)00259-0 ↗
38. Tension and fatigue behavior of a PVD TiN-coated material10.1016/S0040-6090(97)00707-4 ↗
39. Diamond like carbon film as a protective coating for high strength steel and titanium alloy10.1016/j.surfcoat.2006.05.046 ↗
40. Fatigue properties of a 316L stainless steel coated with different TiN x10.1016/S0257-8972(01)01346-9 ↗
41. Effect of the deposition and thickness parameters of titanium nitride (TiN) coatings on the fatigue strength10.1007/s11223-010-9255-8 ↗
42. Fatigue behavior of (graded) (Ti, Al)N-coated 1Cr11Ni2W2MoV stainless steel at high temperature10.1016/j.surfcoat.2010.01.013 ↗
43. Evaluating the effects of plasma diffusion processing and duplex diffusion/PVD-coating on the fatigue performance of Ti-6Al-4V alloy10.1016/j.ijfatigue.2011.04.004 ↗
44. Fatigue properties of a 316L stainless steel coated with different ZrN deposits10.1016/S0257-8972(03)00808-9 ↗
45. Effect of intrinsic properties of ceramic coatings on fatigue behavior of Cr-Mo-V steels10.1016/S0257-8972(03)00229-9 ↗
46. Cavitation erosion of CrN/CrCN multilayer coating10.1016/j.wear.2017.06.007 ↗
47. The resistance of S235JR steel to cavitation erosion10.1016/j.wear.2020.203295 ↗
48. Cavitation Erosion–Phenomenon and Test Rigs10.1515/adms-2017-0028 ↗
49. Slurry Erosion–Design of Test Devices10.1515/adms-2017-0007 ↗
50. Slurry erosion of steel – Review of tests, mechanisms and materials10.1016/j.wear.2018.05.010 ↗
51. Construction of database on cavitation erosion and analyses of carbon steel data10.1016/j.wear.2004.07.002 ↗
52. Ding, X., Ke, D., Yuan, C., Ding, Z., and Cheng, X. (2018). Microstructure and cavitation erosion resistance of HVOF deposited WC-Co coatings with different sized WC. Coatings, 8.10.3390/coatings8090307 ↗
53. Warm Spraying of High-Strength Ni-Al-Bronze: Cavitation Characteristics and Property Prediction10.1007/s11666-016-0487-4 ↗
54. Slurry Erosion Resistance of Martenistic Stainless Steel with Plasma Sprayed Al2O3-40%TiO2Coatings10.1016/j.matpr.2017.11.409 ↗
55. Solid particle erosion mechanisms of protective coatings for aerospace applications10.1016/j.surfcoat.2014.08.037 ↗
56. Fatigue strength at a number of cycles of thin hard coated steels with quench-hardened substrates10.1016/0257-8972(94)02356-5 ↗
57. De Interfacial fatigue stress in PVD TiN coated tool steels under rolling contact fatigue conditions10.1016/S0257-8972(98)00466-6 ↗
58. Rolling contact fatigue of surface coatings—A review10.1016/S0043-1648(02)00234-X ↗
59. Stress analysis and microstructure of PVD monolayer TiN and multilayer TiN/(Ti,Al)N coatings10.1016/S0040-6090(03)00067-1 ↗
60. Monolayer TiAlN and multilayer TiAlN/CrN PVD coatings as surface modifiers to mitigate fretting fatigue of AISI P20 steel10.1016/j.engfracmech.2015.01.009 ↗
61. Effects of the thickness of Ti buffer layer on the mechanical properties of TiN coatings10.1016/S0257-8972(03)00243-3 ↗
62. Evaluation of fatigue resistance of a gradient CrNx coating applied to turbine blades10.1016/j.msea.2009.10.014 ↗
63. Impact-wear behaviors of TiN and Ti-Al-N coatings on AISI D2 steel and WC-Co substrates10.1016/j.surfcoat.2003.08.067 ↗
64. Influence of the substrate hardness on the cavitation erosion resistance of TiN coating10.1016/j.wear.2007.02.003 ↗
65. (2009). ASTM G32-09 Standard Test Method for Cavitation Erosion Using Vibratory Apparatus 1, ASTM International.
66. Influence of cobalt content and HVOF deposition process on the cavitation erosion resistance of WC-Co coatings10.1016/j.wear.2017.12.009 ↗
67. Cavitation erosion performance of CrAlYN/CrN nanoscale multilayer coatings deposited on Ti6Al4V by HIPIMS10.1016/j.jallcom.2019.02.238 ↗
68. Structure and cavitation erosion behavior of HVOF sprayed multi-dimensional WC–10Co4Cr coating10.1016/S1003-6326(18)64681-3 ↗
69. Effect of crystalographic texture on cavitation wear resistance of as-cast CuZn10 alloy
70. On the definition of cavitation intensity10.1016/j.ultsonch.2020.105141 ↗
71. The transient characteristics of cloud cavitating flow over a flexible hydrofoil10.1016/j.ijmultiphaseflow.2017.10.006 ↗
72. Relationship between material pitting and cavitation field impulsive pressures10.1016/j.wear.2016.01.019 ↗
73. Localized Tissue Surrogate Deformation due to Controlled Single Bubble Cavitation10.1007/s11340-015-0024-2 ↗
74. Soyama, H. (2020). Cavitation peening: A review. Metals, 10.10.3390/met10020270 ↗
75. Effect of cavitation intensity on degradation of X6CrNiTi18-10 stainless steel10.1016/j.wear.2018.05.015 ↗
76. Cavitation protection by low temperature TiCN coatings
77. Microstructure and cavitation erosion behavior of sputtered NiCrAlTi coatings with and without N incorporations10.1016/j.jmst.2020.02.072 ↗
78. Cavitation erosion resistance of nanocrystalline TiN coating deposited on stainless steel10.1016/j.wear.2008.02.004 ↗
79. Cavitation resistance of Cr-N coatings deposited on austenitic stainless steel at various temperatures10.1016/j.wear.2008.11.002 ↗
80. Cavitation erosion resistance of NiTi thin films produced by Filtered Arc Deposition10.1016/j.wear.2009.01.035 ↗
81. Szala, M., Walczak, M., Pasierbiewicz, K., and Kamiński, M. (2019). Cavitation erosion and sliding wear mechanisms of AlTiN and TiAlN films deposited on stainless steel substrate. Coatings, 9.10.20944/preprints201904.0228.v1 ↗
82. Wear protection potential of TiN coatings for 304 stainless steels used in rotating parts during olive oil extraction10.1016/j.surfcoat.2016.07.067 ↗
83. Investigation concerning the cavitation resistance of TiN coatings deposited on austenitic stainless steel at various temperatures10.1016/j.wear.2007.08.020 ↗
84. Effect of plasma-assisted laser pretreatment of hard coatings surface on the physical and chemical bonding between PVD soft and hard coatings and its resulting properties10.1016/j.apsusc.2020.145342 ↗
85. Influence of CVD and PVD coating micro topography on the initial material transfer of 316L stainless steel in sliding contacts—A laboratory study10.1016/j.wear.2016.12.003 ↗
86. Arc PVD (Cr,Al,Mo)N and (Cr,Al,Cu)N coatings for mobility applications10.1016/j.surfcoat.2019.125046 ↗
87. Evaluation of adhesion and erosion/corrosion resistance of nano-composite and nano-multilayer thin films in molten aluminum alloy10.1007/s42452-019-1299-1 ↗
88. Properties of TiN and CrN coatings deposited at low temperature using reactive arc-evaporation10.1016/0257-8972(95)02597-9 ↗
89. Reducing the macroparticle content of cathodic arc evaporated TiN coatings10.1016/j.surfcoat.2003.08.086 ↗
90. Recent progress in large scale manufacturing of multilayer superlattice hard coatings10.1016/S0257-8972(00)00959-2 ↗
91. The influence of deposition conditions and bilayer thickness on physical-mechanical properties of CA-PVD multilayer ZrN/CrN coatings10.1016/j.matchar.2018.03.048 ↗
92. The influence of TiN coatings properties on cavitation erosion resistance10.1016/j.surfcoat.2009.07.014 ↗
93. Krella, A.K. (2016). Degradation of protective PVD coatings. Handbook of Materials Failure Analysis, Elsevier.10.1016/B978-0-08-100116-5.00016-8 ↗
94. The new parameter to assess cavitation erosion resistance of hard PVD coatings10.1016/j.engfailanal.2010.10.002 ↗
95. Cavitation erosion behavior of nanocomposite Ti-Si-C-N and Ti/Ti-Si-C-N coatings deposited on 2Cr13 stainless steel using a Plasma Enhanced Magnetron Sputtering process10.1016/j.surfcoat.2010.04.012 ↗
96. Cavitation Resistance of TiN Nanocrystalline Coatings with Various Thickness
97. Effect of coating thickness on the tool wear performance of low stress TiAlN PVD coating during turning of compacted graphite iron (CGI)10.1016/j.wear.2019.01.062 ↗
98. Influences of coating thickness on cutting temperature for dry hard turning Inconel 718 with PVD TiAlN coated carbide tools in initial tool wear stage10.1016/j.jmapro.2020.06.010 ↗
99. Effect of PVD film’s residual stresses on their mechanical properties, brittleness, adhesion and cutting performance of coated tools10.1016/j.cirpj.2016.11.003 ↗
100. Cavitation erosion of TiN and CrN coatings deposited on different substrates10.1016/j.wear.2012.11.049 ↗