Catalyzing Carbonization of Polypropylene Itself by Supported Nickel Catalyst during Combustion of Polypropylene/Clay Nanocomposite for Improving Fire Retardancy
Source abstract
Abstract
The combination of clay layers and a supported nickel catalyst promotes char formation of polypropylene (PP) itself in PP nanocomposites during combustion, which improves the flame retardancy of PP nanocomposites.
Only a short abstract or summary was supplied by the source.
Source: openalex_inverted_index · Quality: short
Research context
OpenAlex topics: Flame retardant materials and properties · Polymer Nanocomposites and Properties · Electromagnetic wave absorption materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
State Key Laboratory of Polymer Physics and Chemistry, Changchun Institute of Applied Chemistry, Chinese Academy of Sciences, Changchun 130022, China, and Department of Chemistry, Shanghai University, Shanghai 200436, China
References (19)
Show source-provided references
1. Gilman J. W. · SAMPE J. · 1997 · 33 · 40
2. Gilman J. W. · Chem. Mater. · 2000 · 12 · 186610.1021/cm0001760 ↗
3. Zhu J. · Chem. Mater. · 2001 · 13 · 377410.1021/cm000984r ↗
4. Zanetti M. · Polym. Degrad. Stab. · 2001 · 74 · 41410.1016/S0141-3910(01)00178-1 ↗
5. Zanetti M. · Chem. Mater. · 2002 · 14 · 88110.1021/cm011236k ↗
6. Wagenknecht U. · 2003
7. Lewin M. · Fire Mater. · 2003 · 27 · 110.1002/fam.813 ↗
8. Zhu J. · Chem. Mater. · 2001 · 12 · 464910.1021/cm010451y ↗
9. Gilman J. W. · 2000
10. Zanetti M. · Chem. Mater. · 2002 · 14 · 18910.1021/cm011124t ↗
11. Beyer G. · Fire Mater. · 2001 · 25 · 19310.1002/fam.776 ↗
12. Kashiwagi T. · Polymer · 2004 · 45 · 422710.1016/j.polymer.2004.03.088 ↗
13. Xie R. X. · J. Appl. Polym. Sci. · 2001 · 80 · 118110.1002/app.1202 ↗
14. Alexandre M. · Mater. Sci. Eng. · 2000 · 28 · 110.1016/S0927-796X(00)00012-7 ↗
15. Bartholmai M. · Polym. Adv. Technol. · 2004 · 15 · 35510.1002/pat.483 ↗
16. Bourbigot S. · Polym. Degrad. Stab. · 2004 · 84 · 48310.1016/j.polymdegradstab.2004.01.006 ↗
17. Zanetti M. · Macromol. Rapid Commun. · 2001 · 22 · 17610.1002/1521-3927(200102)22:3<176::AID-MARC176>3.0.CO;2-C ↗
18. Tang T. · Angew. Chem. Int. Ed. · 2005 · 44 · 151710.1002/anie.200461506 ↗
19. Bockhorn H. · J. Anal. Appl. Pyrolysis · 1985 · 8 · 42710.1016/0165-2370(85)80041-3 ↗